| 性能項目 | 試驗條件[狀態] | 測試方法 | 測試數據 | 數據單位 | |
| 物理性能 | 熔體流動速率 | 220℃×10kg | ASTM D-1238 | 75 | g/10min |
| 熔體流動速率 | 200℃×5kg | ASTM D-1238 | 8.5 | g/10min | |
| 比重 | ASTM D-792 | 1.05 | 23/23℃ | ||
| 機械性能 | 洛氏硬度 | ASTM D-785 | 115 | R | |
| IZOD沖擊強度 | 1/8" | ASTM D-256 | 1.9 | ft.lb/in | |
| 彎曲彈性率 | ASTM D-790 | 2.3×104 | kg/cm2 | ||
| 引張強度 | ASTM D-638 | 400 | kg/cm2 | ||
| 引張強度 | ASTM D-638 | 5670 | lb/in2 | ||
| 彎曲強度 | ASTM D-790 | 9070 | lb/in2 | ||
| IZOD沖擊強度 | 1/4" | ASTM D-256 | 1.5 | ft.lb/in | |
| 彎曲強度 | ASTM D-790 | 640 | kg/cm2 | ||
| 伸長率 | ASTM D-638 | 10 | % | ||
| IZOD沖擊強度 | 1/4" | ASTM D-256 | 8 | kg.cm/cm | |
| 彎曲彈性率 | ASTM D-790 | 3.2×105 | lb/in2 | ||
| IZOD沖擊強度 | 200℃×5kg | ASTM D-256 | 10 | kg.cm/cm | |
| 熱性能 | 熱變形溫度 | ASTM D-648 | 99(210) | ℃ | |
| 燃燒性 | File No. E56070 ULC-UL | 1/16"HB | |||
| 維卡軟化點 | ASTM D-1525 | 221 | ℉ | ||
| 熱變形溫度 | ASTM D-648 | 89(192) | ℉ | ||
| 維卡軟化點 | ASTM D-1525 | 105 | ℃ | ||
中國臺灣奇美ABS(丙烯腈丁二烯苯乙烯) PA-756H物性表
- 特性:通用,高流動
- 用途:家用貨品
- 加工方法:注塑
- 參數:熔流率(熔體流動速率):8.8G/10 MIN 比重:1.05無 熔流率(熔體流動速率):75.0G/10 MIN 彎曲強度:640.0KG/CM2 彎曲模量:23000.0KG/CM2
ABS材料特性
ABS樹脂是五大合成樹脂之一,其抗沖擊性、耐熱性、耐低溫性、耐化學藥品性及電氣性能優良,還具有易加工、制品尺寸穩定、表面光澤性好等特點,容易涂裝、著色,還可以進行表面噴鍍金屬、電鍍、焊接、熱壓和粘接等二次加工,廣泛應用于機械、汽車、電子電器、儀器儀表、紡織和建筑等工業領域,是一種用途極廣的熱塑性工程塑料。ABS是由丙烯腈,丁二烯和苯乙烯組成的三元共聚物。英文名為acrylonitrile–butadiene–styrene copolymer,簡稱ABS。ABS通常為淺黃色或乳白色的粒料非結晶性樹脂。ABS為使用泛的工程塑料之一。